The 17-7PH Alloy Condition 'C' Temper Stainless Steel offers exceptional strength and durability with a thickness of 0.0050 inches. Compliant with ASTM-A-693 and AMS-5529 standards, it features a composition including 18% Chromium and 7.75% Nickel, ensuring high corrosion resistance. With a minimum Tensile Strength of 200 ksi and a Yield Strength of 175 ksi, this stainless steel alloy is ideal for applications requiring precision and reliability.
Product Specifications
Composition Maximum Aluminum Composition
1.50 %
Composition Maximum Carbon Composition
0.09 %
Composition Maximum Chromium Composition
18 %
Composition Maximum Manganese Composition
1.00 %
Composition Maximum Nickel Composition
7.75 %
Composition Maximum Phosphorus Composition
0.04 %
Composition Maximum Silicon Composition
1.00 %
Composition Maximum Sulfur Composition
0.03 %
Physical Properties Minimum Elongation In 2 Inch In
1 %
Physical Properties Minimum Hardness
41 Rockwell C
Physical Properties Minimum Tensile Strength
200 ksi
Physical Properties Minimum Yield Strength 02 Percent Offset
175 ksi
Specifications Alloy
17-7PH Stainless Steel Alloy
Specifications Alloy Steel Type
Stainless Steel
Specifications Ams Standard
AMS-5529
Specifications Astm Steel Standard
ASTM-A-693
Specifications Length
Custom
Specifications Temper
Condition 'C' Temper
Specifications Thickness
0.0050 in
Specifications Thickness Tolerance
5 %
Specifications Width
Custom